BENEFICIATION OF LOW GRADE IRON ORE FINES BY MAGNETIZING ROASTING
Iron ore assayed 59.02% Fe, 3.64% alumina, 3.87% Silica and 6.11% LOI. Proximate of coal and iron ore analysis was carried out and the result are shown in Table 1. Iron ore and non coking coal were crushed and ground to proper size. Mineralogical studies of iron ore fines by optical microscope was carried out.